French translation for "nanoindentation"
|
- nanoindentation
- Example Sentences:
| 1. | The nanoindentation values were found to be 36.4 GPa and 34.0 GPa for the (002) and perpendicular planes respectively. Les valeurs obtenues en nanoindentation sont de 36,4 et 34,0 GPa respectivement pour les plans (002) et les plans perpendiculaires. |
- Similar Words:
- "nanohyla marmorata" French translation, "nanohyla nanapollexa" French translation, "nanohyla perparva" French translation, "nanohyla petrigena" French translation, "nanoid" French translation, "nanokaichi domain" French translation, "nanom" French translation, "nanomantinae" French translation, "nanomaterials" French translation
|
|
|